Influence of particle size, cycling rate and temperature on the lithiation process of anatase TiO<sub>2</sub>. Liu, H. & Grey, C., P. Journal of Materials Chemistry A, 4(17):6433-6446, 2016.
Influence of particle size, cycling rate and temperature on the lithiation process of anatase TiO<sub>2</sub> [link]Website  doi  abstract   bibtex   1 download  
A continuous structural change during the (de)lithiation of lithium-ion battery material, anatase TiO 2 , which undergoes a crystal symmetry change, was not found even at high rates.
@article{
 title = {Influence of particle size, cycling rate and temperature on the lithiation process of anatase TiO<sub>2</sub>},
 type = {article},
 year = {2016},
 pages = {6433-6446},
 volume = {4},
 websites = {http://xlink.rsc.org/?DOI=C6TA00673F},
 id = {0807977b-06f7-3ff5-b947-93178d44c5f0},
 created = {2017-03-10T18:29:06.000Z},
 file_attached = {true},
 profile_id = {acecf9ac-a9eb-39c3-b1a6-bdadc9df448a},
 last_modified = {2023-05-15T19:36:33.271Z},
 read = {true},
 starred = {false},
 authored = {true},
 confirmed = {true},
 hidden = {false},
 private_publication = {false},
 abstract = {A continuous structural change during the (de)lithiation of lithium-ion battery material, anatase TiO 2 , which undergoes a crystal symmetry change, was not found even at high rates.},